Viscosity Measured @25° C Brookfield viscometer DVI+ Spindle No.6 RPM 20/* Spindle No. 6 RPM10/** Spindle No. 7 RPM 20 The required quantity is gradually added to cold water under speed stirring, and after complete addition, continue stirring for 1 hour. Leave paste overnight for maximum swelling or 4-6 hrs. filter the paste using nylon or polyester monofilament 160 mesh bolten cloth.
Packing: 25 Kgs. Paper bags with inner liner.
Stoarge : To be stored in dry and cool place.
No | Name | Composition | Type | Dyes | pH | Paste% | CPS |
1 | Hitech CMT 830 ID M | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 6 | 15 000 to 20 000 |
2 | Hitech CMT 830 ID | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
3 | Hitech CMT EM A8 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 60 000 to 65 000 |
4 | Hitech CMT HT 90 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
5 | Hitech CMT RV 80 | CM Tamarind & Starch | Polyester | Disperse / Acid | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
6 | Hitech CMT ST | CM Tamarind | Polyester / Nylon | Disperse / Burm-out | 9.5 - 10.5 | 8 | 28 000 to 33 000 |
7 | Hitech CMT 600 HV | CM Tamarind | Polyester / PC Blend | Disperse / Acid | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
8 | Hitech CMT RV 900 | CM Tamarind | Polyester / Nylon | Disperse / Acid | 9.5 - 10.5 | 9 | 70 000 to 75 000* |
9 | Hitech 840 DAS | CM Tamarind | Polyester / Nylon | Disperse | 9.5 - 10.5 | 8 | 38 000 to 42 000 |
10 | Hitech CMT 45 | CM Tamarind & Starch | Polyester | Disperse | 9.5 - 10.5 | 8 | 40 000 to 45 000 |
11 | Hitech CMT ZW 10 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
12 | Hitech CMT T 90 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 32 000 to 37 000 |
13 | Hitech CMT 7140 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 40 000 to 45 000 |
14 | Hitech CMT 838 EGP | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
15 | Hitech CMT 110 | CM Tamarind & Starch | Polyester | Disperse | 9.5 - 10.5 | 8 | 45 000 to 50 000 |
16 | Hitech CMT 803 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
17 | Hitech CMT 08 | CM Tamarind | Polyester / PC Blend | Disperse / Burm-out | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
18 | Hitech CMT 8 CH | CM Tamarind | Polyester / Nylon | Disperse / Acid | 9.5 - 10.5 | 8 | 35 000 to 40 000 |
19 | Hitech CMT 3 AV | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 10 | 35 000 to 40 000 |
20 | Hitech CMT 108 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 10 | 85 000 to 90 000** |
21 | Hitech CMT 125 | CM Tamarind | Polyester | Disperse | 9.5 - 10.5 | 10 | 1 00 000 to 1 05 000** |
22 | Hitech HET 835 | Hydroxy Ethylated Tamarind | Polyester / Nylon / Acrylic / PC Blend | Disperse / Acid / Cationic / Burm-out | 9.5 - 10.5 | 8 | 32 000 to 38 000 |
23 | Hitech HET 104 | Hydroxy Ethylated Tamarind | Polyester / Nylon / Acrylic / PC Blend | Disperse / Acid / Cationic / Burm-out | 7.5 - 8.5 | 10 | 35 000 to 40 000 |